Build-up. Fresh printable concrete behaves as a yield-stress material whose yield stress grows with rest time, τy(t) = τ0 + A t (Roussel 2018; τ0 = 1000 Pa here, A set by the accelerator slider). A layer that has k fresh layers on top carries the stress σ = ρ g h k, with ρ = 2200 kg/m³.
Collapse. With a von Mises yield criterion for the uniaxially loaded bead the layer yields when σ ≥ √3 τy. If layers are laid every Δt, layer j has age kΔt when k layers sit on it, so the wall survives only if Δt ≥ maxk (ρ g h k − √3 τ0) / (√3 A k), largest at k = N − 1. With τ0 alone, only ⌊√3 τ0/(ρ g h)⌋ layers can stand.
Cold joints. Fresh-on-fresh bonding is full inside an open time Topen = 30 s and then decays, b = exp(−(Δt − Topen)/Tc) with Tc = 40 s (shape after Wolfs et al. and Le et al.); a joint is called good for b ≥ 0.85, cold below, weak below 0.5. The green bar under the slider is therefore [Δtmin, 36.5 s].
Simplifications: a 1.2 m x 60 mm wall of 24 beads; A, Topen, Tc and the 0.1 r² squash used for drawing are illustrative calibrations, not data for a real mix; no buckling, no lateral wall deflection, no temperature or drying, no reinforcement; real interface strength also depends on surface moisture and nozzle pressure. The collapse animation is a visual stand-in.
Running numerical checks...