🔬 Electron-Beam Lithography Lab: Proximity Effect, Dose and Printed Width

2D interactive simulation · educational model

Choose a pattern and change dose, beam blur and backscatter: see how neighbouring features change the printed width.

The science

Electron-beam lithography (EBL). A focused electron beam writes a pattern into a resist film (here a positive resist such as PMMA, where exposed regions dissolve in the developer). Electrons scatter, so the dose actually deposited is the pattern convolved with a point-spread function, usually modelled as a sum of two Gaussians: PSF(r) = 1/(π(1+η)) [ (1/α²) e−r²/α² + (η/β²) e−r²/β² ]. α is the forward-scattering blur (a few to tens of nm), β the back-scattering range (micrometres in silicon at tens of kV) and η the ratio of backscattered to forward energy (~0.5-1 for silicon).

Proximity effect. Neighbouring features add a background dose ≈ η/(1+η) × local pattern density, so a dense grating receives more dose per feature than an isolated line and its gaps can clear or bridge. Correcting this by adjusting the dose per feature is called proximity-effect correction.

Development. The resist is modelled with a contrast curve h = 1/(1 + (d E / D50)γ), where E is the normalised exposure (1 at the centre of a very large pad), d your dose factor and D50 = 0.5; the region with h < 0.5, i.e. d E > 0.5, is treated as developed. For an isolated line of width w without backscatter, E(x) = ½[erf((x+w/2)/α) − erf((x−w/2)/α)], which the check below uses as an independent reference.

Honest simplifications. The field is a periodic 800 nm tile; the back-scatter range is shown at tile scale (real silicon values are micrometres, giving a larger but smoother background), Gaussian rather than measured PSFs, no secondary-electron blur, no resist swelling or pattern collapse, no stochastic shot noise. All constants are illustrative.