cycles 0 rev.product fraction 0 gWi 11 kWh/t
ChargingSample and ball charge are loaded into the standard mill.
The science

Bond (1952): the energy to grind from feed size F80 to product size P80 (80% passing, in micrometres) is W = 10 Wi (1/√P80 − 1/√F80). Wi is measured in the standard locked-cycle ball-mill test (12″×12″ mill, 700 cm³ feed, 250% circulating load) and computed from the steady-state net grams per revolution Gbp.

Wi = 44.5 / ( P1^0.23 * Gbp^0.82 *
      (10/sqrt(P80) - 10/sqrt(F80)) )   [kWh/short ton]
W  = 10 Wi (1/sqrt(P80) - 1/sqrt(F80))
dW/dx = -K x^-1.5,  K = 5 Wi     (Bond's third law)
P80 ~ 0.75 P1 (typical)   metric: Wi x 1.102 = kWh/t

Simplifications: the cycle-to-cycle Gbp response is modelled as a damped oscillation to the steady value with 1% noise (a real test has hand-sieving error); the test stops when the last three cycles lie within ±3% of their mean. Equation constants are Bond's published ones; ore hardness is your input, not measured.

Independent checks: