Quartz thermal shock - 2D cross-section

A hot plate is dropped into water: the surface contracts first and is pulled into tension until it may crack.

Switch to 3D

Presets

Playback

Material

Plate and quench

A thin plate in strong cooling feels the largest surface stress.

Model checks

The science

Transient conduction

The temperature obeys ∂T/∂t = α ∂²T/∂x² with convective faces -k ∂T/∂x = h (T - Tw), solved implicitly on a half plate with a symmetric mid-plane. The time scale is τ = l²/α with l the half thickness.

Thermal stress

For a free plate the biaxial stress is σ(x) = E αL / (1 - ν) · (Tavg - T(x)): the cold surface is stretched, the hot core squeezed, and the force over the thickness is zero. A very fast quench of ΔT gives the ideal limit σ = E α ΔT / (1 - ν), so the critical shock is ΔTc = σf (1 - ν) / (E α): about 70 K for quartz but over 1000 K for fused silica.

Honest simplifications: constant properties, thin-plate elasticity without edge effects, one fixed strength per material (real strength is statistical and flaw-controlled), no crack growth model, and the alpha-beta inversion of quartz at 573 C (a sudden volume change that adds stress) is only marked, not modelled. Crack drawings are schematic. Material numbers are textbook round values.

What to try
  • Compare Hot quartz into water with the gentle air-cool preset: the same plate survives slow cooling.
  • Switch to fused silica at the same 180 K drop: its low expansion keeps the stress tiny.
  • Use the third graph to see how stress saturates once h is large enough.
Temperature through half the plate now
Surface and centre stress vs time
Peak surface stress vs heat transfer