Battery Electrode Additive Percolation

When does a carbon network connect, and what does it cost in capacity?

Switch to 3D

Presets

Playback

Electrode mix

How much of the solid volume is conductive additive.

Charging

Current density sets the ohmic voltage drop.

Actions

Draw a different random electrode.

Layers

Model checks

The science

The electrode as a voxel grid

The electrode is a 16 x 16 x 16 grid. Each voxel is either conductive additive (carbon-black-like nanoparticles) with probability p or active material. Two voxels that share a face are in contact. The random numbers are fixed for a given electrode, so raising p only adds voxels.

Percolation

Connected groups of additive voxels are clusters. For site percolation on a simple cubic lattice the infinite cluster first appears at p_c = 0.3116 (Lorenz and Ziff 1998). In a finite sample the probability of a connected path from the current-collector side to the other side jumps from near 0 to near 1 over a narrow window around p_c, and the window gets narrower as the grid grows (last graph).

Conductivity

Every contact between two additive voxels is a unit conductance. With potential 1 on the collector layer and 0 on the far layer, Kirchhoff's current law at each interior voxel gives sum over neighbours (V_i - V_j) = 0. The page solves this linear system by successive over-relaxation, sums the current through a mid-plane I and reports sigma = I (L - 1) / L^2 relative to a solid block (1.0). Real conductivity is that value times the carbon network value (taken as 2000 S/m). Near threshold it rises roughly like (p - p_c)^t with an exponent of about 2.

Capacity and loss

Active material only works if electrons can reach it, so an active voxel counts as wired when it touches the spanning additive cluster. Usable capacity is the share of the electrode volume that is wired active material: it climbs steeply above p_c and then falls again because more additive means less active material. The ohmic drop across the electrode is Delta V = J t / sigma for current density J and thickness t = 80 micrometres. Charge carriers on the page hop to lower-potential neighbours with probability proportional to the voltage step.

Simplifications

Voxels are equal cubes, contacts are perfect and equal, only electronic conduction is modelled (no ion transport, no contact resistance between particles, no binder), real electrodes use rod and sheet additives that percolate at lower loadings than random spheres, and the carbon network conductivity is a round number. The percolation numbers are exact for the model; the absolute volts are illustrative.

What to try
  1. Start at 40 % additive: a cyan path crosses the grid. Read the conductivity and the voltage drop.
  2. Press the 25 % preset: only isolated clusters, no path, conductivity zero.
  3. Slide the additive share from 30 to 36 %: the spanning path appears and the conductivity grows from nothing.
  4. Press the 60 % preset: the conductivity is high but the capacity bar falls because less active material is left.
  5. Compare the capacity graph with the conductivity graph and find the additive share that gives the most usable capacity.
Spanning cluster and conductivity against additive share
Usable (wired) capacity against additive share
Ohmic voltage drop against current density
Probability of a connected path for three grid sizes