The Kroll process reduces titanium tetrachloride with liquid magnesium in a sealed, argon-filled steel retort at about 800–900 °C:
TiCl4 + 2 Mg -> Ti + 2 MgCl2 (strongly exothermic)
mass per 1 kg Ti: 3.96 kg TiCl4, 1.02 kg Mg -> 3.98 kg MgCl2
- The Ti forms a porous sponge on the retort wall and over the Mg pool; liquid MgCl₂ is denser than Mg, collects at the bottom and is tapped periodically. If it is not, it floods the retort and feeding must stop.
- Below the Mg melting point (650 °C) the reaction barely proceeds; the model ramps conversion up between 650 and 780 °C. Unreacted TiCl₄ vapour is lost to the scrubber.
- Reaction heat (about 5.2e2 kJ per mol Ti, rounded) is balanced against furnace coupling and wall loss with a first-order lumped model (T_core = T_furnace + Q/5 kW/K at steady state). Hot spots above ~950 °C risk iron pick-up from the steel and sintering of the sponge.
- Vacuum separation at ~1000 °C then evaporates the leftover Mg and MgCl₂ (recycled to magnesium electrolysis). Real sponge keeps a few tenths of a percent of residues; here they are removed completely.
Honest simplifications: lumped single-temperature retort, one-step kinetics, an invented 1-tonne Mg charge, no gas-phase or crust-growth detail. The mass balance is exact stoichiometry.