Why metal breaks below its strength
A load that is far too small to break a part once can break it after many repetitions. Fatigue has two stages: initiation of a tiny crack at the surface or at a stress concentrator, then propagation of that crack a little more on every cycle until the remaining ligament can no longer carry the load.
Stage 1: Basquin S-N life
sigma_a = sigma_f' (2N)^b gives the cycles N to initiate a crack for a fully reversed stress amplitude sigma_a. Mean stress is handled with the Smith-Watson-Topper parameter sigma_eq = sqrt(sigma_max sigma_a), which makes tension harmful and compression helpful. Notches act through the fatigue notch factor Kf = 1 + q (Kt - 1) with Peterson sensitivity q = 1/(1 + a_n/r), and rough surfaces through a knock-down ks. Steels have a knee near 106-107 cycles below which the model reports run-out; aluminium and titanium do not, so run-out is declared at 109 cycles. Damage is summed linearly with Miner's rule, D = N/N_init.
Stage 2: Paris crack growth
da/dN = C (Delta K)^m with Delta K = Y Delta sigma sqrt(pi a). Only the tensile part of the cycle opens the crack, so Delta sigma = sigma_max - max(sigma_min, 0). The geometry factor for a single edge crack in a finite-width plate is the Tada polynomial Y(x) = 1.12 - 0.231x + 10.55x^2 - 21.72x^3 + 30.39x^4, x = a/W. Below the threshold Delta K_th a crack arrests. Final fracture happens when K_max = Y sigma_max sqrt(pi a) reaches the fracture toughness K_Ic or when the net-section stress sigma_max W/(W - a) reaches the flow stress, whichever comes first. For constant Y and m != 2 the life has the closed form N = (a_c^(1-m/2) - a_0^(1-m/2)) / (C (1 - m/2) (Y Delta sigma sqrt(pi))^m).
What is simplified
Material constants are typical handbook values, not certified data. Plasticity at the crack tip, load-sequence effects, the R-ratio dependence of the threshold, corrosion fatigue and the scatter of real S-N data (a factor of 2-10 in life) are not modelled. Low-cycle behaviour above yield uses the elastic Basquin line and is only indicative. Visual stretch of the specimen is exaggerated. Educational model, not for design.
What to try
- Load the Infinite life preset, then raise the amplitude by 20 %: life drops by orders of magnitude (the slope of the S-N curve is only about b = -0.08).
- Add a notch (Kt 2) or a corroded surface and watch the equivalent stress point move up the S-N curve.
- Compare tensile and compressive mean stress at the same amplitude.
- Open the fracture surface: each ring is the crack front after 7 % growth, so the rings crowd together early and spread out late as da/dN accelerates.