Glass Fracture (Griffith)

The science

Griffith/Irwin fracture: a surface flaw of depth a makes the glass fail at sigmaf = KIc / (Y sqrt(pi a)), with fracture toughness KIc = 0.75 MPa m1/2 and geometry factor Y = 1.12 for a shallow edge flaw. Deeper flaws mean much weaker glass.

Stored elastic energy density u = sigma²/(2E) (E = 70 GPa) is released at fracture; a fraction eta (assumed 10%) becomes shard kinetic energy: v = sigma sqrt(eta/(E rho)), rho = 2500 kg/m³. Crack speed is capped well below the Rayleigh wave speed (about 3.3 km/s; real cracks in glass reach about 1.5 km/s).

Simplifications: the shard pattern is a random Voronoi-like layout rather than computed crack branching, glass is perfectly brittle and elastic, shards fly ballistically (display scale 10 units = 1 m) and bounce with damping on the floor.