⚡MYSIMULATORGalvanic corrosion laboratory
Scenario synced
Simulation module · experiment

Timed experiment bench

Run a virtual immersion experiment. A configurable electrolyte salt pulse changes conductivity for a defined interval; dissolved oxygen follows a modest 14-day cycle. The same electrochemical solver calculates every time step.

Experimental protocol

Configure an environmental disturbance, then play the experiment.

60 days
25
12
1.8×
Ready · 0 days elapsed

Live experiment traces

Galvanic current and cumulative mass loss update as the simulation advances.

Galvanic current (mA)

Cumulative metal loss

Metal A loss (g)Metal B loss (g)

Live measurements

Elapsed time0 d
Current—
A cumulative loss—
B cumulative loss—
The model holds the electrode geometry constant and assumes uniform corrosion over the exposed area. The salt pulse changes solution conductivity, not the metal's intrinsic material constants.