Each blow delivers the kinetic energy of the hammer. A fraction of it does plastic work on the metal under the face; the harder the metal (the colder it is), the less it moves. The bar keeps its volume, so every millimetre lost in thickness shows up as length and a little width. Between blows it cools by radiation and convection, and when it falls below the reheat temperature it goes back in the fire.
Equations
- Blow energy
E = ½ m v2; plastic workη E = σf Vd εgives the strain of the blow. - Flow stress
σf(T) = 50 MPa · exp(−(T − 1100 C)/270 K), an illustrative curve for hot steel. - Volume
h b L = const:h → h e−ε,L → L e0.8ε,b → b e0.2ε. - Lumped cooling
ρ c V dT/dt = −A [ hc(T − Ta) + εrσ(T4 − Ta4) ].
Checks run in the page
- The bar volume is unchanged after forty blows.
- Splitting one blow into 200 small ones gives the same thickness.
- Convective cooling follows the exponential solution.
- Radiative cooling follows the exact 1/T^3 solution.
Honest simplifications
The bar is treated as one uniformly worked lump, strained by the fraction of its volume under the face. Flow stress ignores strain rate and strain hardening, the cooling is lumped with constant properties, and the anvil contact is neglected. It shows the trends a smith feels, not a forging process design.
What to try
- Press Narrow face and compare the strain per blow with the wide face.
- Press Cold bar, early reheat and count how many reheats the job needs.
- Lower the reheat limit until the flow stress doubles and the blows stop doing much.