Chemistry. Celestite (SrSO₄) + carbon gives strontium sulfide (“black ash”): SrSO₄ + 2C → SrS + 2CO₂. Above about 1000 K the Boudouard reaction C + CO₂ ⇄ 2CO converts the CO₂: with K = pCO²/pCO2 = exp(−ΔG°/RT), ΔG° = 170.7 − 0.1745 T kJ/mol, the CO mole fraction solves x²/(1 − x) = K; a fraction ψ = x/(2 − x) of the sulfate's 2 CO₂ ends as CO and each sulfate uses 2 + 2ψ carbon (about 4 at kiln temperature). The net reaction is endothermic by about 540 kJ/mol (rounded formation enthalpies).
Kiln transport. A rolling bed advances π D tanβ / sinθr per turn, so τ = L sinθr/(π D N tanβ); at 10 m, 1.2 m, 1.5 rpm, 3 % this is 34 min, within 4 % of the rule of thumb 0.19 L/(N D S).
Bed temperature and conversion. The bed follows the counter-current gas, dT/dt = (Tgas − T)/th (th grows with the fill beyond 10 %). Conversion obeys the contracting-sphere law dX/dt = 3k(1 − X)2/3, k = A exp(−Ea/RT)/r0, closed form 1 − (1 − kt)³; reaction stops when the carbon is used up.
Illustrative parameters. Ea = 210 kJ/mol, A = 8.1 m/s, heating time 240 s, the gas profile and default carbon ratio 4.4 give a plausible kiln, not a fitted plant. Reality depends on coal reactivity, ore grade, gangue and kiln design.
Honest simplifications. Plug flow, single grain size, no gangue, melting, sintering or SrS reoxidation, no flame or heat-loss model (the gas temperature at the burner end is an input), thin-bed transport formula. The kiln section is a Blender render and carries no data; the drawing is a fixed 10 m schematic. Educational chemistry engineering, not a process recipe.
Independent checks (run on load; the same core drives the 3D page):
| running… |