Rule of mixtures (Voigt / iso-strain): loaded along the fibers, fiber and matrix stretch by the same strain, so stiffness adds by volume: E₁ = VfEf + VmEm. Loaded across the fibers (Reuss / iso-stress), they carry the same stress instead, so compliances add: 1/E₂ = Vf/Ef + Vm/Em — a much softer result dominated by the weak matrix.
- Off-axis stiffness: at an angle θ between the load and the fiber axis, classical laminate theory gives 1/Eθ = cos⁴θ/E₁ + sin⁴θ/E₂ + (1/G₁₂ − 2ν₁₂/E₁)·sin²θcos²θ. The cos⁴θ term means stiffness falls off a cliff within the first 10–20° of misalignment — real laminates are stacked at multiple angles for exactly this reason.
- Anisotropic strength: along-fiber failure is set by the strong, stiff fiber; cross-fiber failure is set by the weak matrix (and the stress concentrations it suffers around each fiber), so the same material can be many times stronger in one direction than the other.
Simplifications: a single unidirectional lamina in plane stress, linear elastic up to failure. E1 and E2 are the Voigt and Reuss estimates; the real transverse modulus is a little higher (Halpin–Tsai). Failure strains are illustrative values (fibre strain-to-failure; transverse failure taken as 35% of the neat-matrix strain to mimic stress concentration), and the off-angle failure strain is an empirical 1/ε interpolation, not a Tsai–Hill or Tsai–Wu criterion. There are no voids, residual stresses or fibre waviness. The ply textures are Blender renders; the mechanics is live.
Independent checks: running...