The illustrative specimen is a 120 mm wide steel plate under sinusoidal tensile stress. Its edge crack is treated as straight and through-thickness. For a sufficiently short edge crack, the textbook approximate geometry factor is Y = 1.12.
ΔK = Y Δσ √(πa)
Kmax = Y [Δσ / (1 − R)] √(πa)
da/dN = C(ΔK)³
Here a is crack length in metres, N is load cycles, and K is in MPa√m. The illustrative exponent is 3. With constant Y, let A = C(Y Δσ√π)³; then da/dN = Aa3/2. The exact branch used to advance the model is:
a(N) = [a₀⁻¹ᐟ² − AN/2]⁻²
N(a₁→a₂) = (2/A)(a₁⁻¹ᐟ² − a₂⁻¹ᐟ²)
Below an illustrative 5 MPa√m ΔK threshold the crack is arrested. The model stops at Kmax = KIC (predicted fracture) or a/W = 0.20 (illustrative validity boundary), whichever comes first. Neither threshold nor fracture event is a microscopic damage model.
Simplifications: constant Y is only an approximation for short edge cracks; no finite-width correction, overload history, plastic-zone growth, closure, residual stress, corrosion, changing microstructure or statistical scatter. The vibrating clamps, shiny steel and visible crack opening are illustrative, not a stress-field solution. Cycling is scaled in real time. The three audits test model arithmetic, not whether a particular steel meets the law.
Independent educational model. Not affiliated with any testing-equipment manufacturer or materials supplier.