Laser powder melt pool - 2D thermal field

Plan view and cross-section of a moving laser heat source in four alloys. Conduction-mode Rosenthal model.

Switch to 3D

Presets

Playback

Material

Thermal conductivity and melting point change the pool a lot.

Laser

Power, speed and absorptivity set the heat input.

Layer and hatch

The pool must reach below the powder layer and overlap its neighbour.

Layers

Model checks

The science

Rosenthal moving point source

For a point source of absorbed power Q = η P moving at speed v over a semi-infinite solid, the steady temperature in the moving frame is T = T0 + Q / (2 π k R) · exp(-v (R + ξ) / (2 α)), with R = √(ξ² + y² + z²), thermal diffusivity α = k / (ρ cp) and ξ the distance ahead of the source. The melt pool is the region where T exceeds the melting point Tm; the cooling rate on the trailing melt line is 2 π k v (Tm - T0)² / Q.

Process window

Volumetric energy density E = P / (v h t) (h hatch, t layer). The pool must be deeper than the layer (else lack of fusion) and wide enough to overlap its neighbour; a very deep, narrow pool signals keyhole-prone conditions.

Honest simplifications: point source in a solid half-space: no powder-bed conductivity, latent heat, keyhole recoil, Marangoni flow or temperature-dependent properties, so absolute sizes carry large uncertainty (tens of percent) and the very hot region near the source is exaggerated; use the trends, not the numbers, for real parameter choices. Material values are textbook round numbers.

What to try
  • Standard 316L, then halve the power: the depth drops below the layer line.
  • Raise speed and watch the pool turn into a long, thin tail.
  • Switch to AlSi10Mg: high conductivity needs far more power.
Pool width and depth vs laser power
Pool width and depth vs scan speed
Surface temperature behind the laser