The science
The field. A uniformly magnetised cylinder has the same field as a sheet of current K = Br / mu0 running round its side. The model adds up 56 rings of that current with the exact elliptic-integral field of a loop, so the filings show the real field, not a sketch. On the axis the sum collapses to the closed form Br/2 [(z + L)/sqrt((z + L)^2 + R^2) - z/sqrt(z^2 + R^2)], used as a check. Far away the magnet behaves as a point dipole, m = Br V / mu0.
Pull force. The force between two rigid magnets follows from the poles on their faces, F = (Br / mu0) [Phi(z_a) - Phi(z_b)], where Phi is the flux of the first magnet through a face disc. A magnet on a very permeable steel plate is attracted exactly as if a mirror magnet sat behind the plate, so the force at a gap g is the pair force at separation 2 g. At contact a long magnet gives the textbook B^2 A / 2 mu0 with B = Br. A thin plate cannot carry all the flux: when the flux per plate cross-section exceeds the saturation of steel (1.8 T) the force drops by (B_sat pi D t / Phi)^2. That factor is an estimate with the flux taken from the field of the magnet and its image; real plates saturate gradually. Catalogue pull forces for a 20 x 10 mm N42 disc are lower than the contact value shown (surface roughness, plating, finite plate size), so treat the numbers as an ideal upper estimate.
Temperature. Remanence falls by about 0.12 % per kelvin (reversibly) and the coercivity Hcj by about 0.5 to 0.6 % per kelvin, so the margin to demagnetisation shrinks when it gets hot. The demagnetising field at the centre of the magnet is mu0 Hd = -Br (1 - L / sqrt(L^2 + 4 R^2)): a thin disc is loaded much harder than a long bar. Irreversible loss is taken to start when |Hd| reaches 90 % of Hcj. This is a rule of thumb: edges and corners see a larger field than the centre, so a real magnet starts to lose strength earlier; the grade numbers (Br, Hcj, catalogue limits) are typical catalogue values, not a specific supplier. The model does not simulate the loss itself.
Drop test. The magnet released from rest above the plate accelerates under gravity plus the pull, m dv/dt = F(g) + m g. The kinetic energy at impact equals the integral of that force over the gap, which is one of the checks. The drop is shown in slow motion because the whole fall takes a few milliseconds; air drag is ignored.
Simplifications. Uniform magnetisation (no demagnetisation inside the material), steel plate treated as infinitely permeable except for the saturation estimate, no eddy currents, plating and glue gap ignored, filings are drawn on a regular grid and turned along the computed field direction (real filings clump into lines). The magnet, plate, glass sheet and filings are Blender models; the check at the bottom compares the baked sizes with the reference dimensions.