Peirce-Smith Converter Blow: Fe-Ni-Cu-S Matte Oxidation, Fayalite Slag and Heat Balance

A half-cut Peirce-Smith converter: blast bubbles rise from the tuyeres through the glowing matte under a slag layer while an SO2 plume leaves the mouth. Drag to orbit.

Switch to 2D
Controls

Presets

Parameters

Quality

Camera

Model checks

The science

What a converter does. A nickel-copper matte from the smelter is a molten mixture of iron, nickel and copper sulfides (FeS, Ni3S2, Cu2S). In a Peirce-Smith converter, air is blown through a row of tuyeres below the melt surface. Iron has the strongest affinity for oxygen, so it is burned first: FeS + 3/2 O2 → FeO + SO2. Silica sand is added so that the iron oxide dissolves in a liquid fayalite slag, 2 FeO + SiO2 → Fe2SiO4, which is poured off. The blow stops when the iron has dropped to a few percent (a Bessemer matte); going on would oxidise nickel itself, Ni3S2 + 7/2 O2 → 3 NiO + 2 SO2, and lose it to the slag. The sulfur leaves as SO2 in the off-gas.

Model. A 100 t charge is tracked in kilomoles. Oxygen is shared between FeS and Ni3S2 in proportion to n(FeS) and kappa n(Ni3S2), where kappa is a deliberately illustrative selectivity constant. Heat comes from the three reactions, using reaction enthalpies built from rounded standard formation enthalpies (FeS, FeO, SO2, Ni3S2, NiO, SiO2, Fe2SiO4); it leaves with the hot exhaust gas, through the shell and mouth (one lumped loss coefficient), and in heating the cold flux and cold matte revert that operators add to keep the bath from overheating. The temperature follows from C dT/dt = Q_reaction - Q_gas - U (T - 25) - Q_flux - Q_revert with a variable bath heat capacity.

What the checks compare. (1) An element ledger for Fe, Ni, S and O over a blow with flux and revert, against the oxygen drawn from the blast. (2) The temperature integrated with the composition held fixed against the closed form T_inf + (T0 - T_inf) e^(-t/tau), plus the full model's initial slope against a hand-assembled coefficient set. (3) The Ni3S2 inventory against the exact power law (n_Fe/n_Fe0)^(3 kappa/7) that follows from the oxygen split. (4) The blow time to the target iron against the closed-form lever rule, since iron removal is linear in time when the oxygen all goes to iron.

Simplifications. Thermochemical data and heat capacities are handbook-level roundings at 298 K or mean values, not a calibrated plant model. Real converters have non-equilibrium kinetics, slag and matte mutual solubility (so some nickel and copper always reports to slag), magnetite and viscosity limits, tilting of the vessel and dust. The selectivity kappa and the loss coefficient are illustrative. This is an educational model of the physics and not an operating guide.