ELECTROCHEMISTRY × GEOMETRY INTERACTIVE FIELD NOTES
Cut your own electrode. Switch on the cell. Discover how charge becomes copper — and how the surface you design changes its coating.
Move copper rivets to redraw the metal. Every grid step is 0.25 cm. A changed shape starts a fresh run.
The curve is generated from accumulated electric charge. Change current mid-run to change its slope.
The copper anode connects to positive; the workpiece is the negative cathode. The DC supply drives reduction and oxidation.
Model: constant current within each adjustment; 100% current efficiency; a dissolving copper anode; copper(II) ions do not become depleted; perfectly uniform plating on both faces; thin, flat conductive substrate; edge area, surface roughness, current crowding and side reactions neglected. Thickness is average, not a local prediction.
Constants: Faraday constant F = 96,485.33212 C mol⁻¹; copper molar mass M = 63.546 g mol⁻¹; copper density ρ = 8.96 g cm⁻³. Copper requires two electrons per ion.
Used for: decorative finishing, printed circuit features, protective coatings and electrorefining. In a real tank, shape affects current distribution and therefore coating uniformity; bath composition, agitation, electrodes and safety precautions matter.