Black Mass Leaching: Stirred Acid Tank, Shrinking Cores and Heat-Up

A steam-heated stirred tank dissolves lithium, cobalt, nickel and manganese from battery black mass: shrinking-core kinetics, stirring power, solids suspension and acid balance.

Switch to 2D

Presets

Playback

Parameters

Camera

Layers

Quality

Model check

The science

What is modelled

Recycling plants shred spent lithium-ion cells into a dark powder called black mass (graphite plus nickel, manganese and cobalt oxides and lithium compounds) and dissolve the metals in hot sulfuric acid, usually with hydrogen peroxide as a reducing agent. The page follows one batch in a stirred, steam-heated tank: the tank warms up, the acid attacks the particles from the outside in, and the slurry changes from black to a coloured solution.

Equations

  • Shrinking core under mixed control (surface reaction plus diffusion through the product layer): t = tau_r [1 - (1-X)^(1/3)] + tau_d [1 - 3 (1-X)^(2/3) + 2 (1-X)], which gives dX/dt = 1 / (tau_r / (3 u^(2/3)) + 2 tau_d (u^(-1/3) - 1)) with u = 1 - X. Each of Li, Co, Ni and Mn has three particle size classes.
  • Temperature: tau scales with exp[Ea/R (1/T0 - 1/T)] (Ea = 42 kJ/mol for the reaction, 18 kJ/mol for diffusion); the reaction time falls as acid strength to the power -0.6; Co and Mn dissolve slowly without peroxide.
  • Stirring: P = Np rho N^3 D^5 for a Rushton turbine (Np = 5), pumping Q = Nq N D^3, circulation time V/Q, particle mass transfer Sh = 2 + 0.52 (eps d^4/nu^3)^0.2 Sc^(1/3) with eps = P/(rho V), and the just-suspended speed of Zwietering, N_js = S nu^0.1 d_p^0.2 (g drho/rho)^0.45 X^0.13 D^-0.85. Below N_js only a fraction of the solids take part.
  • Heat-up: C dT/dt = UA (T_steam - T) + P - UA_loss (T - Ta); hydrogen peroxide decays as exp(-k t) with an Arrhenius k.
  • Acid is consumed stoichiometrically by every mole of metal dissolved and can run out.

Checks run in the page

  • The mixed-control closed form against RK4 and a numerical dt/dX integral.
  • Acid consumption equals the stoichiometric sum over a whole batch.
  • The initial rate ratio against the Arrhenius law.
  • Heat-up and peroxide decay against their exponentials.
  • Power cube law, power number, Sherwood limits and Reynolds regime.
  • Blender geometry against the model dimensions.

Honest simplifications

The metal contents, rate constants and activation energies are illustrative and chosen to give leaching times of the order of hours, not fitted to a particular black mass; real extraction depends on the cathode chemistry, pre-treatment, the graphite and binder, and on impurities such as aluminium and copper. The particle size distribution is three fixed classes, the slurry viscosity is that of water, the same tank mixing is assumed everywhere and the suspension factor is a simple power law. Hydrogen peroxide is not consumed by the reduction itself and the reactions are not coupled through the common acid beyond the acid balance. The grains drawn in the tank follow two idealised circulation loops of the right pumping rate and shrink with the computed extraction; they are not a flow simulation. Educational model, not a plant design tool.

What to try

  • Switch off the peroxide: lithium and nickel still dissolve, cobalt and manganese stall.
  • Drop the stirrer to 45 rpm: below the just-suspended speed part of the solids rests on the floor and the batch slows.
  • Compare 30 C and 90 C in the third graph: the time to 90 percent falls by an order of magnitude.
Loading model...
Loading Blender model...
Metal extraction against time
Slurry temperature, acid and peroxide
Time to 90 percent extraction against temperature
Made with 🟠 Blender · Three.js