Feldspar Flotation Cell, Side Section

2D twin of the 3D flotation cell: the same first-order rate model and checks, with Blender-rendered cell parts seen from the side.

Switch to 3D

Presets

Playback

Flotation conditions

Air flux, bubble size, collector, pH and froth depth set the rate constants; flotation time is the clock of the 10-minute test.

Run

Model checks

The science

What you see. A laboratory froth-flotation cell separating feldspar from quartz after the mica has already been floated off. An impeller disperses air into fine bubbles; collector-coated grains stick to them, ride up into the froth and spill over the weir into the concentrate pan. Raise the air flux, change the bubble size, the amine dosage, the pH and the froth depth, run the 10-minute test and watch recovery, grade and the alkali content.

Rate of flotation. In a batch cell the amount left in the pulp falls as exp(−k t), so recovery is R(t) = 1 − exp(−keff t). The true flotation rate constant is built from the bubble surface-area flux Sb = 6 Jg/db and three probabilities: k = η · (1/4) Sb Pc Pa Ps (Gorain et al.). Collision Pc = (3/2 + 4Re0.72/15)(dp/db)² (Yoon & Luttrell) makes fine grains float slowly. Attachment Pa = exp(−tind/tslide) compares the induction time with the time a grain slides along the bubble. Stability Ps = 1/(1+(dp/dmax)4) uses the largest grain the capillary force can hold against its (turbulence-enhanced) weight, dmax = √(6σ sin²(θ/2) / (ψ Δρ g)), so coarse grains drop off. The bubble rise speed comes from a numerical balance of buoyancy and Schiller–Naumann drag.

Chemistry in the model. Feldspar is floated with a cationic amine collector in an HF-acidified pulp near pH 2–3; quartz is depressed there and floats instead in the alkaline amine window (pH 7–10). The contact angle follows a Langmuir collector coverage times a pH window. Entrainment of fine gangue follows the water recovery, which rises with air flux and falls with froth depth, and the froth recovery exp(−0.18 h) models drop-back from a deeper froth.

Honest simplifications. The efficiency η = 0.05, the induction-time law, the contact-angle window, the froth-recovery constant, the drop-back and entrainment laws and the five size classes are illustrative calibrations that reproduce the known trends (a recovery peak at intermediate size, a pH window, a grade–recovery trade-off with froth depth), not measured data for a particular ore. First-order kinetics with a single rate per size class ignores the distribution of floatability inside a class, the changing pulp density and air hold-up, and the bubble loading limit. Bubbles in the picture are drawn three times larger than the chosen size and rise at about a third of their true speed so they can be seen. Hydrofluoric acid is a hazardous reagent used only in industrial plants.

Checks. (1) a Monte Carlo of 20 000 grains against the analytic recovery; (2) the rise-speed solver against Stokes' law; (3) mass balance plus the maximum floatable size found by scanning the force balance; (4) the Stokes-flow limit of the collision probability and the linear scaling of the rate with air flux.

What to try
  • Press Run test and watch the recovery curves climb while loaded bubbles carry grains into the froth and over the weir.
  • Set the pH to 9: quartz now floats as well and the concentrate grade collapses.
  • Set collector to 0: only water-entrained fines reach the froth.
  • Deepen the froth: the grade rises and the recovery falls (last graph).
  • Use large bubbles (2.5 mm): the surface-area flux Sb = 6 Jg / db drops and so does the rate constant.
Recovery and grade against flotation time
Recovery by particle size (collision and detachment)
Result after 10 minutes against pulp pH
Result after 10 minutes against froth depth
Made with 🟠 Blender